This guide covers component-specific sample preparation within the Lab Sample Preparation workflow. Depending on the target market and age grading, laboratory evaluation commonly includes EN 71 mechanical and chemical assessment under the EU Toy Safety framework, alongside material declarations for packaging compliance such as VerpackG and Triman / Info-Tri when finished retail boxes accompany the boards.
Specifications and Sample Conditions
Laboratory samples must replicate the exact substrate thickness, adhesive chemistry, lamination film, and mechanical fasteners used on the production line.
| Component Type | Core Greyboard & Tolerances | Wrap, Film & Die Specs | Required Sample State |
|---|---|---|---|
| Folding Boards & GM Screens | 1.5 mm, 2.0 mm, 2.5 mm, or 3.0 mm (0.059 in, 0.079 in, 0.098 in, or 0.118 in) | 15–20 mm (0.591–0.787 in) wrap margin; double-sided film adds 0.03–0.05 mm (0.0012–0.0020 in) | Fully wrapped, creased, and cured; hinge tape or wrap joints intact |
| Dual-Layer Boards | Multi-ply greyboard (e.g., 1.5 mm / 0.059 in base + 1.5 mm / 0.059 in recessed top) | Full-surface or perimeter adhesive lamination; 3 mm (0.118 in) bleed and >=3 mm (0.118 in) safety | Top and bottom plies permanently bonded; cutouts aligned and cured |
| Punchboards & Die-Cut Puzzles | 1.5–2.5 mm (0.059–0.098 in) greyboard | 3–4 mm (0.118–0.157 in) die gap between adjacent tokens; anti-scuff matte suits dark art | Sheets unpunched with all retaining nicks intact; separate loose tokens only if requested |
| Spinners & Dial Boards | 2.0–3.0 mm (0.079–0.118 in) greyboard | Coated wrap stock (distinguish US Text LB on 25 x 38 in basis sheet from Cover LB on 20 x 26 in basis sheet when specifying gsm) | Metal or plastic dial rivets clinched at production torque; washers seated |
Unit conversion reference: inches = millimetres / 25.4 (for example, 2.0 mm / 25.4 = 0.079 in).
Job-Specific Preparation Steps
Produce with final substrates and wrap adhesives Build test boards using the exact multi-ply greyboard caliper, CMYK + spot ink build, lamination film, and cold or hot-melt wrap glue specified for the production run. Hand-glued prototypes or unlaminated digital prints omit the adhesive and film layers required for chemical extraction and edge-peel assessment.
Preserve punchboard nicks and die-cut bridges Leave all tokens, tiles, and puzzle pieces seated in the waste frame with production nicks intact. Labs inspect how cleanly tokens separate, whether nicks leave sharp fibrous burrs, and whether detached pieces trigger small-parts cylinder checks.
Install and cure dial rivets and dual-layer bonds Clinch all eyelets, rivets, and rotating dials using production dies, and allow dual-layer board adhesives to reach full cure before packing. Rivets installed by hand pliers or uncured dual-layer laminates shift under tension and torque testing.
Pack flat with material documentation Stack boards and punchboards flat with protective interleaving so transit friction does not scuff matte coatings or snap punchboard nicks. When shipping packed sets, maintain standard box clearance—1.5–2.5 mm (0.059–0.098 in) across width/height and 1.5–3.0 mm (0.059–0.118 in) for stack height—and attach a bill of materials listing greyboard ply, wrap gsm (with Text/Cover basis), adhesive type, film type, and fastener alloy or polymer.
Sign-Off Criteria
Verify the following physical conditions before dispatching samples to the testing laboratory:
- Adhesive cure and flatness: Wrap margins of 15–20 mm (0.591–0.787 in) are fully bonded around corners with zero edge lifting, bubbling, or delamination between dual-layer plies.
- Intact nicks: 100% of punchboard tokens and puzzle pieces remain held in the sheet by their die-cut nicks after packing.
- Hardware seating: Dial rivets rotate smoothly without tearing the paper wrap or cracking the underlying greyboard.
- Print and coating match: Surfaces carry the exact production varnish or film (such as anti-scuff matte on dark artwork) rather than an uncoated proof finish.
- Complete material record: Every layer—greyboard, wrap paper, adhesive, ink, coating, and rivet—is identified by material class for chemical and packaging-record matching.
Concrete Failure Modes
- Pre-punched tokens or broken nicks: Shipping loose tokens or sheets with snapped nicks prevents the lab from evaluating separation force and edge burrs, and can cause premature small-parts failures during transit simulation.
- Substitute or uncured wrap glues: Using temporary spray mount or unaged PVA instead of production wrap glue leads to corner delamination during thermal/humidity conditioning and distorts chemical migration results.
- Hand-cut dual-layer recesses: Cutting recesses manually instead of using the production steel-rule die leaves inconsistent 3–4 mm (0.118–0.157 in) bridges and rough inner edges that fail mechanical edge-integrity checks.
- Improperly clinched dial rivets: Under-clinched rivets detach during pull and torque testing, creating a small-parts hazard; over-clinched rivets crush the greyboard core and split the surface wrap.
- Missing lamination on dark or folded edges: Omitting the 0.03–0.05 mm (0.0012–0.0020 in) film layer masks hinge cracking on folding boards and GM screens, invalidating repeated-flex durability results.
Parent guide Preparing Representative Paper and Non-Paper Lab Samples
Related guides
- Preparing Resin Dice and Acrylic Game Piece Samples
- Preparing Foil Boosters, Shrink Wrap, and Packaging Film Samples
- Preparing Printed Cards, Booklets, and Coated Paper Samples
- Preparing Gilded-Edge and Foil-Stamped Card Samples
- Preparing Die-Cast Metal Coin Samples
- Preparing Neoprene Playmats and Drawstring Pouch Samples