This guide covers coin-specific sample grouping within the broader lab sample preparation workflow.
Material and Finish Variables
Testing laboratories evaluate both the underlying metal substrate and every accessible surface layer. Prepare samples around the exact production variables that alter chemical composition or mechanical edge geometry:
- Zinc-Alloy Base Substrate: Die-cast game coins typically use zinc-alloy castings. Because laboratories screen for restricted heavy metals in both coatings and base metal, submitted coins must come from the production alloy lot rather than substitute prototyping metal.
- Electroplating Baths: Bright brass, copper, nickel, gold-tone, and black-nickel finishes use different plating chemistries and barrier layers. Nickel-containing underplates or topcoats also affect nickel-release testing, so every plating bath must be submitted separately.
- Antique Washes and Topcoats: Oxidizing or darkening washes, tumbling residues, and protective clear lacquers change surface chemistry and wear behavior. An antiqued finish cannot be represented by a bright plated coin of the same base metal.
- Enamel Fills: Soft and hard enamel fills use separate resin binders and colorant pigments. Every enamel color used across a coin set must appear in the submitted samples so pigment screening covers all colorways.
- Dimensions and Mass Records: Record each coin's actual diameter and thickness in mm (in) and unit or sample-lot weight in kg (lb) on the sample manifest, since size and mass determine small-parts and surface-area handling during assessment.
Sample Preparation Steps
- Pull from Production-Representative Tooling and Finishing: Collect coins after final die-casting, tumbling, deburring, plating, washing, and enamel curing on the production line. Avoid hand-filed or hand-buffed pre-production pieces that mask normal parting-line flash or tumble-finish wear.
- Segregate by Finish Combination: Bag and label each unique combination of alloy lot, electroplating bath, antique wash, and enamel color separately. Do not mix multiple finishes in one bag.
- Attach Material Declarations: Include alloy composition certificates, plating bath specifications, and enamel pigment safety data sheets with the physical samples. Where toy or age-graded tabletop rules apply, reference European Commission Toy Safety (EN 71) assessment and testing procedures alongside the target market's chemical and mechanical requirements.
- Pack to Prevent Transit Abrasion: Place coins in individual compartments or foam-lined trays with desiccant so edges and faces do not strike each other during shipping.
Sign-Off Criteria
- Every production plating bath, antique wash, and enamel colorant in the order is represented by finished, labeled samples.
- Each sample bag maps directly to a documented alloy lot and finishing batch on the manifest.
- Coins arrive free of shipping scratches, chipped enamel, or cross-contamination between finishes.
- Laboratory reports confirm acceptable base-metal screening, surface plating release, and mechanical burr/edge inspection before bulk finishing or box assembly begins.
Concrete Failure Modes
- Submitting One Representative Finish: Testing only a bright-plated coin and skipping an antique or black-nickel variant leaves different plating baths and surface washes unverified, invalidating coverage for the untested finishes.
- Sending Unplated Blanks Alone: Raw zinc-alloy castings omit plating chemistries, antique washes, and enamel pigments that govern surface-contact and release results.
- Hand-Deburred Prototypes: Manually smoothed samples hide sharp casting flash, rough parting lines, and edge burrs that occur under standard mass-production tumbling cycles.
- Omitted Enamel Colors: Leaving even one enamel colorant out of the lab submission blocks verification for coins carrying that pigment and forces supplemental testing.
- Bulk-Bagging Loose Coins: Shipping loose coins together abrades thin clear coats, chips enamel fills, and introduces transit nicks that trigger false mechanical or surface-release failures.
Parent guide Preparing Representative Paper and Non-Paper Lab Samples
Related guides
- Preparing Game Boards, Dual-Layer Boards, and Punchboard Samples
- Preparing Foil Boosters, Shrink Wrap, and Packaging Film Samples
- Preparing Printed Cards, Booklets, and Coated Paper Samples
- Preparing Resin Dice and Acrylic Game Piece Samples
- Preparing Gilded-Edge and Foil-Stamped Card Samples
- Preparing Neoprene Playmats and Drawstring Pouch Samples