Conditions That Change Sample Grouping
The exact sample count and breakdown depend on how your components are molded, cut, and decorated:
- Single-color vs. swirled or layered resin: A solid-color resin die needs one base polymer group. Multi-color swirled, marbled, or layered resin dice require sampling each distinct pigment mixture used in the pour, unless the manufacturer confirms all swirls share a single base resin and separate colorant concentrates are supplied for screening.
- UV-printed acrylic vs. raw laser-cut acrylic: Unprinted tinted acrylic tokens are tested as homogeneous plastic. Adding CMYK + white UV-printed artwork introduces surface coatings and photoinitiators that must be tested separately from the cast or extruded acrylic sheet.
- Recessed pip paint and metallic fills: Dice with engraved or recessed pips filled with acrylic enamel, lacquer, or metallic paint require liquid paint samples or cured paint plaques alongside the finished dice, because scraping tiny pip cavities rarely yields enough coating mass for chemical extraction.
- Standee bases and multi-part assemblies: Acrylic standees paired with separate slotted bases, protective peel-off films, or glued overlays require each distinct plastic thickness, adhesive, and film layer to be itemized on the sample manifest.
Material and Coating Specifications
| Component Layer | Production Process | Lab Sample Requirement | Key Preparation Detail |
|---|---|---|---|
| Base cast resin | Silicone-mold casting, tumbling, polishing | Undecorated resin blanks per tint | Group by base resin formula and pigment batch; remove polishing compounds before packing |
| Acrylic sheet | Laser-cut cast or extruded PMMA | Unprinted cut blanks per sheet tint and thickness | Strip protective paper or film unless the film remains on the retail piece |
| Surface UV ink | Flatbed UV-curable inkjet printing (CMYK + white) | Printed flat swatches and finished tokens/standees | Print full-coverage ink swatches on the same acrylic substrate when token art has low ink area |
| Recessed pip paint | Spray-and-wipe or needle-fill enamel | Finished painted dice plus cured paint drawdowns | Supply wet or cured paint plaques when recessed pips hold minimal paint volume |
| Edges and corners | Laser kerf, flame polish, or barrel tumbling | Finished production-edge pieces | Submit pieces after final tumbling or edge finishing, not raw off-the-cutter parts |
When providing flat ink swatches or sheet blanks, keep acrylic sheet thicknesses consistent with production—for example, 3.0 mm (0.118 in) standees or 2.0 mm (0.079 in) tokens—and record component mass in both g/kg and oz/lb on the sample manifest if the lab requires minimum extraction weights.
Job-Specific Preparation Steps
- Lock the component bill of materials (BOM) before pulling samples. List every resin colorant, acrylic sheet batch, UV ink set, clear topcoat, and pip paint used across the set. Exclude packaging components from the piece manifest unless the lab is evaluating the complete retail box.
- Pull undecorated base blanks from the active batch. Set aside unprinted acrylic cutouts and unpainted, uninked resin dice casts from the exact resin pour and sheet lot used for production. Label each bag with the material code and color name.
- Prepare high-coverage ink and paint surrogates where surface area is small. If UV artwork covers only a thin border or dice pips are narrow, have the manufacturing partner print solid 100% coverage patches of each UV ink channel on scrap acrylic, and cure drawdowns of each pip paint on an inert backing.
- Apply final mechanical finishing to physical check samples. Tumble resin dice and polish or deburr laser-cut acrylic standees using the exact production cycle. Labs run sharp-edge, sharp-point, and small-parts checks on finished geometry, not unpolished blanks.
- Pack each material family in separate, sealed bags. Do not mix different resin tints, UV-printed variants, or painted dice loose in a single pouch; pigment transfer or UV ink abrasion during transit skews surface extraction.
Sign-Off Criteria and Regulatory Context
For markets requiring toy or juvenile product compliance, EN 71 assessment and testing evaluate mechanical hazards (such as small parts, sharp edges on laser-cut acrylic corners, and drop/impact integrity) alongside chemical migration from polymers and surface coatings. Procedures and official guidance for European toy safety compliance are maintained by the European Commission on its Toy Safety in the EU portal.
Lab submission sign-off requires:
- Complete material traceability: Every finished piece maps to a documented resin tint, acrylic sheet lot, ink set, and pip paint record in the BOM.
- Sufficient mass per homogeneous group: Each distinct polymer and surface coating meets the lab's minimum sample weight or surface area without forcing technicians to combine different colors.
- Verified final surface state: Protective masking films are removed (unless shipped to end users with film intact) and tumbling/polishing residues are washed off.
- Conditional record retention: Test reports and material declarations apply only to the exact formulations and manufacturing processes submitted; any subsequent change to resin supplier, UV ink batch, or laser-cut edge finish requires re-evaluation.
Concrete Failure Modes
- Pip paint contamination in polymer tests: Submitting only finished, inked resin dice leaves the lab unable to isolate pure resin without grinding away pip cavities, risking false chemical failures or invalid extraction weights.
- Insufficient coating mass on fine-line UV prints: Submitting only tokens with thin line art forces the lab to request additional units mid-test, delaying approval. Always include solid-coverage UV ink drawdowns for low-coverage designs.
- Uncured or tacky UV ink: Under-cured UV prints transfer ink onto adjacent standees or bag walls during shipping, causing cross-contamination and coating adhesion failures.
- Sharp laser-cut acrylic corners: Unchamfered 90-degree laser-cut standee tabs or cracked acrylic slots can fail mechanical sharp-edge checks; specify edge rounding or polishing before pulling lab samples.
- Leftover polishing compound on resin dice: Tumbled dice shipped with residual wax or abrasive paste introduce external compounds into surface-wipe or migration tests. Wash and dry resin samples thoroughly before bagging.
Parent guide Preparing Representative Paper and Non-Paper Lab Samples
Related guides
- Preparing Wooden Meeples and Painted Wood Piece Samples
- Preparing Game Boards, Dual-Layer Boards, and Punchboard Samples
- Preparing Rigid, Two-Piece, and Magnetic Box Samples
- Preparing Foil Boosters, Shrink Wrap, and Packaging Film Samples
- Preparing Printed Cards, Booklets, and Coated Paper Samples
- Preparing Gilded-Edge and Foil-Stamped Card Samples