Material Grouping and Component Specifications
Accredited laboratories separate a finished game into homogeneous materials—each distinct substrate, ink system, coating, adhesive, or polymer/pigment batch that can be mechanically separated for testing. Grouping components accurately before shipment prevents labs from re-cutting mixed stacks or rejecting insufficient specimen mass.
When recording paper weights for lab submission forms, list both metric grammage (gsm) and the corresponding US basis weight, distinguishing US Text LB (basis sheet 25 x 38 in / 635 x 965 mm) from US Cover LB (basis sheet 20 x 26 in / 508 x 660 mm), since the same gsm converts to a different pound weight depending on the basis sheet.
| Component Group | Representative Substrates & Caliper | Coating, Ink & Assembly Variables | Lab Grouping Rule |
|---|---|---|---|
| Offset Card Stock | 300 gsm art/blue core (0.28–0.31 mm / 0.011–0.012 in); 310 gsm black-core linen (0.30–0.32 mm / 0.012–0.013 in); 330 gsm black core (0.32–0.34 mm / 0.013 in); 350 gsm art stock (0.34–0.38 mm / 0.013–0.015 in); 400 gsm (0.40–0.44 mm / 0.016–0.017 in) | CMYK with TAC <= 280%–300%, separate spot layers, anti-scuff matte varnish, or double-sided film (+0.03–0.05 mm / +0.001–0.002 in per card); gilded edges | Group by identical core stock, ink set, and surface finish; separate plain-edge decks from gilded-edge decks |
| PVC Card Stock | 0.30 mm (0.012 in) rigid PVC | Offset UV or screen-printed CMYK plus spot layers and protective varnish | Isolate from paper card stocks; group by PVC sheet batch and ink/varnish system |
| Booklets & Leaflets | Interior 80–120 gsm (about 54–81 lb US Text, 25 x 38 in / 635 x 965 mm; 0.08–0.13 mm / 0.003–0.005 in per sheet); covers 200–300 gsm (about 74–111 lb US Cover, 20 x 26 in / 508 x 660 mm) | Saddle-stitch wire staples (12–40 pages), perfect-binding EVA/PUR spine glue (28+ pages), or sewn thread (80–100+ pages) | Submit bound copies plus loose unprinted/printed interior and cover sheets; separate staples and adhesives |
| Rigid Boxes, Boards & Punchboards | 1.5 mm (0.059 in), 2 mm (0.079 in), 2.5 mm (0.098 in), or 3 mm (0.118 in) greyboard | Wrapped printed paper (15–20 mm / 0.591–0.787 in wrap margin), laminating glue, anti-scuff matte or gloss film, punchboard die-cut edges (3–4 mm / 0.118–0.157 in die gap) | Provide both finished assembled boxes/boards and raw greyboard + printed wrap + adhesive components |
| Partner-Sourced Non-Paper Pieces | Molded plastic trays/miniatures, wooden tokens, resin/acrylic dice, metal coins | Masterbatch colorants, surface paints, pad-printed inks, or clear coats | Group strictly by material type, pigment/color batch, and surface coating; never mix colors in one bag |
Job-Specific Sample Preparation Steps
Lock the Bill of Materials (BOM) Before Pulling Confirm that the offset press sheets, box wraps, and partner-sourced components match the approved production specifications. Verify that prepress files used for the press run—exported from AI/PDF/PSD as PDF/X-1a or PDF/X-4 with outlined or embedded fonts, 100% K fine text, and rich black (C40–60 M30–40 Y30–40 K100) within TAC <= 280%–300%—match the actual plates on press.
Pull From Cured Offset Press Runs and Finishing Lines Collect card decks, punchboards, and booklets after ink drying, varnish or film lamination curing, and die-cutting. For standard offset runs starting at 200 decks (and typical 200/300/500/1,000+ tiers), pull samples from the middle of the stabilized press run rather than initial make-ready sheets so ink density and fountain solution balance represent shipped inventory.
Separate Raw Substrates From Finished Assemblies When a component combines multiple materials—such as a 2 mm (0.079 in) greyboard rigid box wrapped in laminated art paper, or a perfect-bound rulebook—ask the manufacturing partner to supply both finished units and unglued raw subcomponents (blank greyboard, unlaminated/laminated press sheets, dry adhesive pellets or cured glue films). This allows labs to test individual layers without scraping contamination between substrates.
Isolate Non-Paper Batches by Pigment and Finish For partner-sourced game pieces (plastic inserts, wooden cubes, dice, tokens), pull samples from the exact production lot and color masterbatch scheduled for assembly. Separate unpainted pieces from painted or pad-printed pieces so coating tests can be run independently of the base polymer or wood.
Weigh and Record Packaging vs. Product Components Measure finished component and packaging weights on calibrated scales in both kg and lb (for example, recording a 0.45 kg / 0.99 lb box assembly separately from a 0.12 kg / 0.26 lb card deck). Accurate production weights and material breakdowns support packaging registration and sorting-mark filings where applicable, such as Germany's VerpackG packaging register and France's Info-tri / Triman labeling records.
Bag, Label, and Ship With Traceability Seal each homogeneous group in clean, unprinted polyethylene bags so printed outer cartons or tape adhesives do not transfer onto test surfaces during transit. Label each bag with the component name, material spec (gsm / US Text or Cover LB, caliper in mm/in), coating or colorant ID, production batch number, and gross sample weight (kg/lb).
Sign-Off Criteria
Before releasing samples to an accredited laboratory—whether for general chemical screening or toy-safety assessment and testing such as EN 71 under the EU Toy Safety framework—verify all of the following gates:
- Process match: Every paper and card sample is offset-printed and finished with the exact production varnish, film, or edge treatment (no digital or POD stand-ins).
- Cure completeness: Lamination, UV spot coatings, and box-wrap adhesives are fully cured with no residual solvent odor or tackiness.
- Homogeneous separation: Each distinct core stock, ink/spot-layer family, and non-paper colorant batch is bagged and labeled separately.
- Mass and surface area sufficiency: Sample quantities provide enough uniform surface area and weight (kg/lb) for the lab to take multiple test cuts without mixing batches.
- Documentation parity: The sample packing list matches the production BOM, including exact gsm, basis weight type (Text LB vs. Cover LB), caliper (mm/in), and packaging material weights.
Concrete Failure Modes
- Submitting digital prototypes as production proxies: Digital presses use electrophotographic toners or UV-curable inkjet inks instead of offset vegetable/mineral inks and aqueous/UV varnishes. Test results from digital mockups do not transfer to offset runs and require re-testing once the press run finishes.
- Pooling mixed paper cores or finishes: Bagging 300 gsm blue-core cards together with 330 gsm black-core cards or gilded-edge variants forces the lab to either reject the batch or run separate unquoted extractions, delaying sign-off.
- Sampling uncured make-ready sheets: Pulling sheets before ink and lamination adhesives cure traps volatile compounds inside sealed sample bags, skewing extraction readings and causing film delamination during lab cutting.
- Assuming one non-paper color represents all pigments: Testing only a natural wood or white plastic piece omits heavy-metal or restricted-substance risks carried by specific red, yellow, blue, or metallic masterbatch pigments and surface paints.
- Using estimated packaging weights: Estimating tuck-box or rigid-box weights from CAD templates rather than weighing die-cut greyboard (1.5–3 mm / 0.059–0.118 in) and finished wraps creates discrepancies in producer-responsibility filings and shipping manifests.
Guides in this section
- Preparing Game Boards, Dual-Layer Boards, and Punchboard Samples
- Preparing Foil Boosters, Shrink Wrap, and Packaging Film Samples
- Preparing Printed Cards, Booklets, and Coated Paper Samples
- Preparing Resin Dice and Acrylic Game Piece Samples
- Preparing Gilded-Edge and Foil-Stamped Card Samples
- Preparing Die-Cast Metal Coin Samples
- Preparing Neoprene Playmats and Drawstring Pouch Samples
- Preparing Card Sleeves, Blister Trays, and EVA Foam Samples
- Preparing PVC and Plastic Card Samples for Chemical Testing
- Preparing Rigid, Two-Piece, and Magnetic Box Samples
- Preparing Wooden Meeples and Painted Wood Piece Samples
Parent guide Safety Testing and Environmental Verification
Related guides
- Preparing Conformity Declarations and Statutory Safety Markings
- Documenting Certified and Recycled Paper Sourcing Claims
- Collecting Partner Material Declarations Before Lab Testing
- Checking Lab Test Reports Against the Production Specification
- Age Grading and Intended-Use Screening for Test Planning
- Documenting Packaging Material Disclosures and Environmental Claims