Within the broader lab sample preparation workflow, this choice depends on whether components share a single paper core and surface finish or combine distinct substrates, adhesives, and coatings. When a game or deck mixes black-core card stock, coated booklet signatures, folding carton board, and adhesive stickers, each unique material stack must be submitted in finished form alongside matching documentation.
Sample Specifications and Material Grouping
Testing laboratories evaluate either composite finished pieces (substrate + ink + coating) or separated layers depending on the requested protocol, such as EN 71 assessment and testing under the EU Toy Safety framework for youth-oriented games. Group your submission by physical stack rather than by artwork file so every chemical and mechanical layer is represented.
| Component Type | Typical Stock & Caliper | Ink, Coating & Layer Considerations |
|---|---|---|
| Offset Playing & Game Cards | 300 gsm art/blue core (0.28–0.31 mm / 0.011–0.012 in), 310 gsm black-core linen (0.30–0.32 mm / 0.012–0.013 in), 330 gsm black core (0.32–0.34 mm / 0.013 in), 350 gsm art stock (0.34–0.38 mm / 0.013–0.015 in), 400 gsm (0.40–0.44 mm / 0.016–0.017 in) | Double-sided film lamination adds 0.03–0.05 mm (0.001–0.002 in) per card and introduces polymer film and adhesive layers. Include gilded edges or anti-scuff matte finishes if used in production. |
| Booklets & Paper Inserts | Interior: 80–120 gsm (0.08–0.13 mm / 0.003–0.005 in per sheet; US Text LB on a 25 × 38 in / 635 × 965 mm basis sheet). Covers: 200–300 gsm (US Cover LB on a 20 × 26 in / 508 × 660 mm basis sheet) | Submit both cover and interior stocks when paper grades or coatings differ. Note binding format: 4/6/8-panel leaflets, saddle stitch (12–40 pages), perfect binding (28+ pages), or sewn binding (80–100+ pages). |
| Folding Tuck Boxes | Paperboard matched to box dimensions and stack clearance | Include external varnish, spot UV, or matte lamination, plus any glued seam adhesive used on the folding carton. |
| Paper Stickers & Labels | Coated or uncoated face stock with release liner | Must be submitted intact so the lab can account for face ink, topcoat, and pressure-sensitive adhesive. |
Ink and Surface Coverage Requirements
- Full-coverage CMYK and rich black: Select cards or press sheets that carry maximum ink density—up to the 280%–300% total area coverage (TAC) ceiling—including rich black builds (C40–60 M30–40 Y30–40 K100) and 100% K fine text.
- Separate spot layers: If the prepress package (AI, PDF, or PSD exported as PDF/X-1a or PDF/X-4) uses Pantone, metallic, or fluorescent spot plates, every spot ink must appear on the submitted samples.
- Surface finishes: Aqueous varnish, UV coating, anti-scuff matte film, and edge treatments alter surface extractables and abrasion behavior; never substitute uncoated proofs for coated production runs.
Step-by-Step Sample Preparation
- Audit the Bill of Materials and Prepress Separations Cross-check the production spec sheet against the PDF/X-1a or PDF/X-4 layers to list every unique paper stock, core glue, ink channel, varnish, film lamination, and binding adhesive.
- Source Press-Matched Finished Pieces Pull finished samples from a production run or a wet press proof made with the exact offset inks, varnishes, and laminating films. Because standard offset card runs start at 200 decks (200 / 300 / 500 / 1,000+ tiers), early compliance checks can use dedicated press-proof sheets cut and finished to match production tolerances (such as 3 mm / 0.118 in bleed and R3–R3.5 mm / 0.118–0.138 in corners where applicable) before committing to full-quantity finishing.
- Include Raw Unprinted Stock When Requested If the testing lab separates substrate analysis from surface-coating analysis, pack a small quantity of unprinted, unvarnished base stock from the same mill lot alongside the finished printed samples.
- Cure, Bag, and Weigh by Material Family Allow inks, varnishes, and carton adhesives to cure completely before packing. Seal each material family in a clean, unprinted poly bag labeled with the component name, gsm, and US Text LB or Cover LB basis. For composite chemical or extraction tests that specify minimum sample mass, verify the lab's weight threshold in advance (commonly 0.5–1.0 kg / 1.1–2.2 lb per distinct material group).
Sign-Off Criteria
Confirm the following before shipping samples to the testing laboratory:
- Complete ink and coating representation: Every CMYK build, spot color, varnish, and film lamination in the job appears on the physical pieces in the parcel.
- Verified stock identity: Paper weights (gsm and correctly distinguished Text LB vs. Cover LB) and caliper measurements match the production order.
- Clean, cured condition: Samples are dry, free of wet-ink transfer, and untouched by permanent markers, tape adhesive, or unapproved packing materials.
- Traceable manifest: Each bagged group maps one-to-one to a line item on the lab submission form listing substrate, ink system, and requested assessment standard.
Concrete Failure Modes
- Submitting blank white stock for printed jobs: Testing unprinted paper misses heavy ink pigments, spot metallics, and surface varnishes, leaving the lab report incomplete for finished goods.
- Sending only light-coverage cards: Cards with minimal artwork under-represent maximum TAC (280%–300%) and rich black ink loads.
- Omitting lamination or sticker adhesives from the manifest: Failing to declare double-sided film (+0.03–0.05 mm / +0.001–0.002 in) or pressure-sensitive adhesives causes labs to misclassify a composite polymer-paper stack as pure paper.
- Confusing US Text LB and Cover LB: Recording a 200–300 gsm booklet cover as Text LB (25 × 38 in) instead of Cover LB (20 × 26 in) creates a paper-grade discrepancy between lab records and production specs.
- Packing uncured or contaminated sheets: Sealing freshly varnished cards or labeling directly onto sample faces with felt-tip markers introduces solvent residues and false test readings.
Parent guide Preparing Representative Paper and Non-Paper Lab Samples
Related guides
- Preparing PVC and Plastic Card Samples for Chemical Testing
- Preparing Game Boards, Dual-Layer Boards, and Punchboard Samples
- Preparing Foil Boosters, Shrink Wrap, and Packaging Film Samples
- Preparing Resin Dice and Acrylic Game Piece Samples
- Preparing Gilded-Edge and Foil-Stamped Card Samples
- Preparing Die-Cast Metal Coin Samples