Sample Preparation Verdict and Changing Conditions

Submit both complete, production-cured boxes and isolated raw sub-components in the same lab kit. Intact boxes validate structural seams, corner stays, hinge durability, and magnet retention under mechanical stress, while loose raw components allow clean chemical, coating, and magnetic flux-index testing without destructive disassembly.

Three conditions change how the sample kit is built:

  • Box construction (two-piece telescoping vs. magnetic flip-top): Two-piece rigid boxes rely on corner stays, wrap tension, and lid-to-base clearance, requiring intact lid and base pairs for drop, crush, and seam-separation checks. Magnetic flip-top boxes add embedded magnets, concealed cavities, and scored spine hinges, requiring both intact hinged units for retention/cycling and loose unmounted magnets for flux-index measurement.
  • Target market and age grading: Boxes packaged with games or toys intended for children require formal EN 71 toy safety assessment and testing covering mechanical hazards, magnet retention, flux index, and restricted substances. Packaging for adult-only tabletop products typically shifts focus toward transit integrity and packaging material records for programs such as VerpackG or Triman sorting instructions.
  • Surface finishes and multi-layer wraps: Uncoated or single-pass printed wraps require fewer chemical test groups than wraps combining inks, lamination, anti-scuff matte coatings, or metallic foils. Each distinct surface layer must be accessible on an unmounted sheet.

For general component grouping and submission rules across all game formats, see Lab Sample Preparation.

Specifications and Component Breakdown

Rigid boxes combine thick structural board with tensioned paper wraps, adhesives, and localized hardware. Record all dimensions, board calipers, and weights on the sample manifest using metric and imperial units together (in = mm / 25.4, lb = kg * 2.205).

Structural and Print Specifications

  • Greyboard caliper: Standard rigid box walls use 1.5 mm (0.059 in), 2.0 mm (0.079 in), 2.5 mm (0.098 in), or 3.0 mm (0.118 in) greyboard.
  • Wrap turn-in margin: Outer wrap paper requires a 15–20 mm (0.591–0.787 in) turn-in folded over the board edge to anchor cleanly to the interior liner.
  • Internal box clearance: Telescoping and hinged boxes use 1.5–2.5 mm (0.059–0.098 in) clearance across width and height and 1.5–3.0 mm (0.059–0.118 in) for stack height; test units must match these production clearances rather than tight hand-fitted mockups.
  • Artwork bleed and safety: Wrap sheets require 3 mm (0.118 in) bleed per side and at least 3 mm (0.118 in) safety margin from fold and score lines so compliance marks and graphics remain intact after wrapping.
  • Paper basis weight logging: Log wrap and interior liner weights in gsm. When referencing US paper weights alongside gsm, distinguish US Text LB (25 x 38 in / 635 x 965 mm basis sheet) from US Cover LB (20 x 26 in / 508 x 660 mm basis sheet) so lab documentation matches the exact sheet specification.

Required Sample Forms

Sample Form Included Materials Primary Test Purpose Key Manifest Details
Intact Assembled Box Complete lid/base or hinged flip-top unit with embedded magnets Corner integrity, hinge cycling, magnet retention, drop/crush Greyboard caliper (mm/in), unit mass (kg/lb), adhesive type
Loose Embedded Magnets Unmounted magnets from the exact production lot Flux-index measurement and small-parts cylinder checks Magnet grade, dimensions (mm/in), unit mass (kg/lb)
Unmounted Printed Wrap Flat wrap sheets with all production inks and coatings (e.g., anti-scuff matte) Surface coating heavy-metal and chemical screening Paper weight (gsm and Text/Cover LB), coating layers
Corner Stays & Hinges Raw gummed stay tape, cloth hinge strips, or spine reinforcements Material composition and seam-bond verification Backing material, adhesive type, width (mm/in)
Adhesive / Glue Lot Sealed wet sample or cured film strip of wrapping and magnet glues Restricted substance and VOC screening Glue chemistry, lot code, cure schedule

Job-Specific Sample Preparation Steps

  1. Lock the production-intent Bill of Materials: Confirm the exact greyboard thickness (1.5–3.0 mm / 0.059–0.118 in), wrap finish, corner-stay material, adhesive chemistry, and magnet placement before pulling lab units.
  2. Produce assembled boxes on production-method tooling: Run test boxes using the actual V-grooving, die-cutting, corner-staying, and wrapping equipment rather than hand-cutting or substituting craft glue. Hand-assembled mockups alter wrap tension over the 15–20 mm (0.591–0.787 in) turn-ins and distort mechanical corner and magnet-retention outcomes.
  3. Pull flat, unmounted wrap sheets from the press run: Set aside printed and coated wrap sheets before they enter the gluing and wrapping line. Labs need uncontaminated surface coatings that have not absorbed board adhesive.
  4. Bag loose magnets and adhesive samples from the same batch: Collect unmounted magnets directly from the assembly feeder rather than prying them out of finished boxes, which chips plating and alters test geometry. Place liquid or cured adhesive samples in sealed, labeled containers with matching batch numbers.
  5. Cure completely before packing: Allow assembled rigid boxes to cure fully in conditioned air before sealing them in polybags. Record individual unit mass and total parcel weight in kg and lb, and pack boxes with rigid corner protectors so parcel transit does not pre-damage the 90-degree edges.

Sign-Off Criteria

A rigid or magnetic box sample kit is ready for lab intake when it meets all four conditions:

  • Full traceability: Every assembled box, wrap sheet, magnet bag, and adhesive vial carries matching batch codes, dimensions in mm (in), weights in kg (lb), and gsm/basis-sheet records tied to the Bill of Materials.
  • Cured structural state: Assembled boxes show flat panels, bonded 15–20 mm (0.591–0.787 in) wrap turn-ins, intact corner stays, and zero transit crush or hinge cracking.
  • Complete component isolation: All homogeneous layers (wrap paper, coatings, corner stays, greyboard, glue, and loose magnets) are present separately so chemical and flux-index testing can proceed without scraping or prying apart finished boxes.
  • Aligned regulatory documentation: Test submission forms map each component to the applicable EN 71 mechanical, magnet, and chemical procedures, and any printed packaging disposal marks match VerpackG or Triman records where required.

Concrete Failure Modes

  • Sending only assembled boxes without loose magnets or raw wraps: Labs are forced to chisel glued magnets out of 2.0–3.0 mm (0.079–0.118 in) greyboard cavities and scrape coated paper off glued board, damaging magnet plating, contaminating coating samples with glue, and delaying test completion.
  • Substituting hand-glued prototypes for production-cured units: Craft glues or hand-pressed wraps cure with different bond strength than production hot-melt or cold-PVA adhesives, causing false passes or unexpected failures in mechanical corner-pull and magnet-retention tests.
  • Sealing uncured boxes in airtight polybags: Trapped moisture and adhesive solvents soften greyboard corners and lift 15–20 mm (0.591–0.787 in) wrap turn-ins during transit, triggering pre-test rejection or premature delamination.
  • Omitting corner-stay tape or spine-hinge strips: Listing only greyboard and wrap paper omits the gummed paper or cloth stays reinforcing the corners and magnetic flap hinge, halting lab intake when unlisted materials appear during teardown.
  • Shipping rigid boxes without corner protection: Crushed corners on 1.5–3.0 mm (0.059–0.118 in) greyboard boxes disqualify the units from baseline drop, compression, and seam-integrity testing.