This guide covers how PP or CPP sleeves, formed PET trays, and EVA foam adhesives change polymer chemical screening and off-gassing sample preparation within the Lab Sample Preparation workflow.
Conditions That Change the Sample Set
The exact number of lab specimens depends on material grade, surface treatment, colorant count, and bonding method:
- Sleeve polymer and finish: Cast polypropylene (CPP) and oriented polypropylene (PP) use different slip and heat-seal additives. Clear glossy sleeves, matte-textured sleeves, tinted backs, and printed or foiled sleeve faces must each be submitted as separate specimens.
- Thermoformed PET tray state: Forming heat, mold-release agents, and anti-static coatings alter surface chemistry. Finished thermoformed trays—not flat unformed PET sheet—are required for every tint, clear grade, or flocked finish.
- EVA foam density and adhesive layers: Each foam color and density requires its own specimen. When multi-layer EVA inserts are laminated with pressure-sensitive adhesive (PSA) or hot-melt glue, both the bonded foam assembly and the adhesive-bearing layer must be represented so volatile residuals and heavy metals in the glue line are screened.
| Component | Material / Process Variables | Required Separate Submissions | Primary Screening Focus |
|---|---|---|---|
| Card sleeves | PP vs. CPP; clear vs. matte/anti-slip; printed or tinted backs | One set per polymer grade, finish, and ink/colorway | Plasticizers, heavy metals, surface coating/ink residuals |
| Blister trays | Clear rigid PET vs. tinted PET; anti-static or flocked surfaces | One formed tray set per resin tint and surface treatment | Plasticizers, heavy metals, forming/release residuals |
| EVA foam inserts | Single-layer vs. laminated multi-layer; PSA or hot-melt glue | One set per foam color/density plus each adhesive layer | Volatile foam residuals (off-gassing), heavy metals, plasticizers |
Where components are part of products subject to toy-safety rules, EN 71 assessment and testing records follow the procedures outlined by the European Commission Toy Safety framework. Where sleeves, blister trays, or protective foam function as sales or transport packaging, component material weights (recorded in kg and lb) and resin/material classifications support conditional reporting under systems such as Germany's Verpackungsregister (VerpackG) and France's Info-Tri (Triman) sorting rules.
Job-Specific Preparation Steps
- Lock the component bill of materials before pulling specimens. List every sleeve film grade, tray resin tint, foam color/density, and adhesive SKU or batch identifier used by Card Deck Press's specialist manufacturing partners.
- Pull production-representative formed and bonded parts. Collect heat-sealed PP/CPP sleeves from the production roll, thermoformed PET trays directly off the production mold (maintaining production box clearances of 1.5–2.5 mm / 0.059–0.098 in across width/height and 1.5–3 mm / 0.059–0.118 in for stack height), and die-cut EVA foam after full lamination and standard curing.
- Isolate each variant to prevent cross-contamination. Seal each colorway, surface finish, and adhesive-backed foam variant in its own clean, unprinted, non-plasticized barrier bag. Never pack freshly cut EVA foam in the same bag as PP/CPP sleeves or PET trays.
- Label specimens with traceability and unit mass. Tag each bag with the component name, polymer/foam type, colorant batch, adhesive identifier, cure time, and single-unit mass in g/kg and oz/lb to align lab screening records with Lab Sample Preparation intake logs and packaging weight declarations.
Sign-Off Criteria
- Every production colorway, matte/anti-static finish, and adhesive layer maps 1:1 to a tested lab specimen without substituting clear or unbonded stock.
- PET tray specimens come from thermoformed production tooling rather than flat sheet stock, and EVA foam specimens reflect production lamination and curing conditions.
- Chemical screening, off-gassing, EN 71 assessment records (where applicable), and component mass records (kg/lb) are filed against the exact production material lot before mass assembly begins.
Concrete Failure Modes
- Transit cross-contamination: Bagging EVA foam inserts together with clear PP/CPP sleeves or PET trays transfers volatile foam residuals onto the films and trays, causing false off-gassing or chemical screening failures on clean polymers.
- Unformed sheet substitution: Sending flat PET sheet instead of thermoformed blister trays omits mold-release agents, anti-static sprays, and heat-forming effects present on finished trays.
- Missing colorant or adhesive layers: Testing only natural/clear EVA or a single sleeve color leaves pigment masterbatches, matte coatings, and PSA/hot-melt lamination adhesives unscreened for heavy metals and plasticizers.
- Unrepresentative foam curing: Pulling EVA samples straight off the laminator traps uncured adhesive volatiles, while leaving samples unwrapped for extended periods before bagging dissipates residuals that would otherwise remain inside a sealed retail box.
Parent guide Preparing Representative Paper and Non-Paper Lab Samples
Related guides
- Preparing Gilded-Edge and Foil-Stamped Card Samples
- Preparing PVC and Plastic Card Samples for Chemical Testing
- Preparing Game Boards, Dual-Layer Boards, and Punchboard Samples
- Preparing Foil Boosters, Shrink Wrap, and Packaging Film Samples
- Preparing Printed Cards, Booklets, and Coated Paper Samples
- Preparing Resin Dice and Acrylic Game Piece Samples