Specifications and Weight Basis
Specify cover stock in gsm alongside its US Cover LB rating so manufacturing partners do not confuse cover caliper with interior text sheets. US Cover LB measures a 500-sheet ream at a 508 x 660.4 mm (20 x 26 in) basis sheet size, whereas US Text LB measures a 500-sheet ream at a 635 x 965.2 mm (25 x 38 in) basis sheet size.
| Property | Uncoated Cover Stock | Interior Pairing (Reference) |
|---|---|---|
| Weight range | 200–300 gsm | 80–120 gsm |
| US basis weight | 74–111 lb Cover, 33.6–50.3 kg per 500-sheet 508 x 660.4 mm (20 x 26 in) ream | 54–81 lb Text, 24.5–36.7 kg per 500-sheet 635 x 965.2 mm (25 x 38 in) ream |
| Sheet thickness | Varies by furnish and texture | 0.08–0.13 mm (0.003–0.005 in) per interior sheet |
| Binding compatibility | Saddle stitch (12–40 pages), perfect binding (28+ pages), sewn binding (80–100+ pages recommended) | Multiples of 4 pages per signature; 4/6/8 panels for unfolded leaflets |
| Prepress files | AI, PDF, or PSD exported as PDF/X-1a or PDF/X-4 | Same prepress standard |
| Resolution and margins | >=300 DPI, 3 mm (0.118 in) bleed per side, >=3 mm (0.118 in) safety | Same prepress standard |
| Ink and black limits | CMYK with separate spot layers, 100% K fine text, rich black C40–60 M30–40 Y30–40 K100, TAC <=280%–300% | Same prepress standard |
Production Steps and Surface Behavior
- Fiber absorption and prepress compensation: Uncoated and textured fibers draw wet offset ink downward into the sheet rather than holding it on a clay-coated top layer. Keep Total Area Coverage (TAC) at or below 280%–300%, use 100% K for fine text, and build dark fills with rich black (C40–60 M30–40 Y30–40 K100) so shadow detail does not plug up from dot gain.
- Dry-rub resistance and curing: Without a sealed coating or film, pigment sits exposed among surface fibers. Allow full oxidative drying time on racked sheets before cutting or folding, and avoid stacking high-coverage covers directly against raw greyboard or unvarnished box liners where vibration causes dry-rub transfer.
- Hinge scoring behavior: Heavy 200–300 gsm uncoated sheets resist sharp 180-degree folds, especially when textured fibers run perpendicular to the spine. Score all cover hinges and spine creases mechanically with a channel matrix before folding, aligning the paper grain parallel to the spine whenever sheet layout permits.
- Surface writability: Open cellulose fibers accept ballpoint pens, pencils, permanent markers, and rubber stamps without smearing. Keep ink coverage light or knocked out to bare paper in designated log boxes, signature lines, and campaign note fields.
Sign-Off Criteria
- Ink density and tone: Wet-proof or press-sheet check confirms shadow separation stays open under TAC <=280%–300% and 100% K micro-type remains crisp against textured valleys.
- Score and fold integrity: Folded cover samples show a clean, uniform hinge with zero fiber cracking along the outer spine or perfect-bound/sewn hinge lines.
- Dry-rub transfer: Rubbing a cured cover face against white paper and adjacent box stock under firm hand pressure produces no visible pigment smearing.
- Writability check: Ballpoint pen and graphite pencil write smoothly across designated note areas without skipping or bleeding through to the inside cover.
Failure Modes
- Ink transfer onto adjacent box pieces: Full-bleed dark backgrounds on uncoated covers scuff against cards, dividers, or box walls during shipping, leaving dark smudges on light components; keep heavy dark solids off contact surfaces or switch to a coated cover with anti-scuff matte lamination.
- Spine and hinge cracking: Folding 250–300 gsm uncoated stock without deep mechanical scoring—or folding cross-grain—fractures surface fibers along the crease, exposing white paper core on printed spines.
- Muddy halftones and plugged shadows: High-TAC artwork (>300%) over-saturates porous fibers, causing tonal compression and slow drying that leads to set-off on the back of stacked press sheets.
- Saddle-stitch spring-back: Pairing a stiff 300 gsm textured cover with a low page count (near 12 pages) causes the booklet to yawn open instead of lying flat inside standard 1.5–3 mm (0.059–0.118 in) box height clearances.
Parent guide Booklet, Leaflet, and Reference Paper Stocks