Specifications and Weight Equivalents
Self-cover jobs replace the standard split between 80–120 gsm interior sheets (about 0.08–0.13 mm / 0.0031–0.0051 in per sheet) and 200–300 gsm covers with one mid-weight sheet. In US paper sizing, basis weights are distinguished by sheet size: US Text LB uses a 25 × 38 in (635 × 965 mm) 500-sheet ream, while US Cover LB uses a 20 × 26 in (508 × 660 mm) 500-sheet ream.
| Metric Weight | US Text LB (25 × 38 in / 635 × 965 mm) | US Cover LB Equivalent (20 × 26 in / 508 × 660 mm) | Practical Self-Cover Role |
|---|---|---|---|
| 105 gsm | ~70 lb Text | ~39 lb Cover | Lightweight manuals (20–40 pages) where low stack height and flat folding matter more than cover stiffness |
| 120 gsm | ~80 lb Text | ~44 lb Cover | Balanced mid-range sheet for 16–32 page manuals needing clean folds without excessive bulk |
| 128 gsm | ~86 lb Text | ~47 lb Cover | Standard offset art-stock choice for 12–28 page rulebooks with full-color spreads |
| 135 gsm | ~90 lb Text | ~50 lb Cover | Firmer outer feel for 12–24 page booklets handled frequently at the table |
| 157 gsm | ~106 lb Text | ~58 lb Cover | Maximum practical self-cover weight; best kept to 12–20 pages to limit spine springback |
Structural, Fit, and Prepress Limits
- Signature & Binding Limits: Bound signatures run in multiples of 4 pages. Saddle stitching covers 12–40 pages total; above 28 pages, evaluate perfect binding (28+ pages) or sewn binding (80–100+ pages) if thickness causes inner-page creep.
- Box Fit & Clearance: Total booklet thickness must fit within the box's 1.5–2.5 mm (0.059–0.098 in) width/height clearance and 1.5–3 mm (0.059–0.118 in) vertical stack clearance alongside cards, boards, and trays.
- File & Color Setup: Supply AI, PDF, or PSD files exported as PDF/X-1a or PDF/X-4 at ≥300 DPI in CMYK with separate spot layers. Embed or outline all fonts, keep fine body text at 100% K, use rich black (C40–60 M30–40 Y30–40 K100) for solid fills, and cap Total Area Coverage (TAC) at ≤280%–300%.
- Margins & Bleed: Include 3 mm (0.118 in) bleed on all outer trim edges and keep critical text and page numbers inside a ≥3 mm (0.118 in) safety margin from the trim line.
- Surface Protection: Dark outer artwork benefits from an inline anti-scuff matte varnish or aqueous coating rather than thick film lamination, which adds 0.03–0.05 mm (0.0012–0.0020 in) per laminated side and increases spine springback.
Job-Specific Production Steps
- Imposition and Grain Alignment: Impose all cover and interior spreads onto a single master form with the paper grain running parallel to the spine fold. Parallel grain prevents fiber cracking along the outer score and keeps the booklet lying flat.
- Single-Form Offset Printing: Print the cover and interior spreads together through the same offset press pass with Card Deck Press manufacturing partners. Maintaining consistent ink density across one stock eliminates color-shift mismatches between the outer wrap and page 2/page 3 spreads.
- Folding, Collation, and Saddle Stitching: Fold the printed 4-page signatures, nest them in page order, and drive two wire staples through the spine crease.
- Creep Compensation and Three-Knife Trim: Apply progressive inner-margin creep compensation on higher page counts (24–40 pages) before executing the three-knife face, head, and foot trim so outer borders remain uniform from the cover to the center spread.
Sign-Off Criteria
- Flat-Lay and Box-Fit Check: The finished booklet rests closed without popping open past 2–3 mm (0.079–0.118 in) at the fore-edge and slides into the game box within the 1.5–2.5 mm (0.059–0.098 in) width/height and 1.5–3 mm (0.059–0.118 in) stack-height tolerances.
- Spine and Staple Integrity: Both wire staples clinch flush against the center spread with no loose legs, and the outer fold shows no white fiber cracking or tearing around the staple holes under normal page turns.
- Trim and Print Registration: All 3 mm (0.118 in) bleeds trim cleanly, ≥3 mm (0.118 in) safety margins hold across inner and outer signatures, and 100% K fine text remains sharp without misregistration halos.
Concrete Failure Modes
- Staple Tear-Out on Thin Stock: Dropping below 105 gsm (or using 80–90 gsm interior paper as a self-cover) leaves insufficient fiber mass under the wire clinch, causing the outer wrap to tear away from the staples during repeated handling.
- Spine Springback and Fore-Edge Creep: Running 157 gsm stock past 24–28 pages builds excessive fold bulk; the booklet springs open inside the box, and inner spreads push outward so the face trim cuts closer to inner-spread margins.
- Cross-Grain Fold Cracking: Folding 135–157 gsm coated sheets perpendicular to the paper grain fractures the coating along the spine crease, leaving visible white stress lines across dark cover solids.
- Outer-Spread Scuffing and Set-Off: Printing heavy dark solids on an uncoated or unvarnished self-cover without anti-scuff matte protection or TAC ≤280%–300% causes ink transfer and rub marks where the booklet contacts cards or box inserts in transit.
Parent guide Booklet, Leaflet, and Reference Paper Stocks