Specifications and Material Behavior
Uncoated tactile and flashcard stocks rely on open, uncalendered or lightly sized paper fibers rather than clay coatings or plastic films. Because there is no sealed top layer, liquid ink penetrates the fiber network and graphite abrades onto the paper tooth.
- Basis Weight and US Paper Scales: Card stock is specified in grams per square meter (gsm). When referencing US pound weights, distinguish Cover LB (based on a 20 × 26 in / 508 × 660 mm basis sheet) from Text LB (based on a 25 × 38 in / 635 × 965 mm basis sheet). Because the Cover basis sheet is smaller, a given Cover LB rating represents a substantially thicker, stiffer board than the same number in Text LB.
- Caliper Reference Tiers: Depending on fiber density and cotton content, card-grade boards sit in the following approximate thickness ranges (compared against standard coated/core baselines):
- 300 gsm: 0.28–0.31 mm (0.0110–0.0122 in)
- 350 gsm: 0.34–0.38 mm (0.0134–0.0150 in)
- 400 gsm: 0.40–0.44 mm (0.0157–0.0173 in)
- Adding double-sided film lamination increases total card thickness by 0.03–0.05 mm (0.0012–0.0020 in) per card, which is omitted on bare writeable stocks.
- Minimum Run: Standard offset card runs start at 200 decks (usual tiers: 200, 300, 500, and 1,000+ decks).
- Prepress and File Tolerances:
- File Formats: AI, PDF, or PSD, exported as PDF/X-1a or PDF/X-4 with outlined or embedded fonts.
- Color and Resolution: CMYK with separate spot layers where required; ≥300 DPI for all raster artwork.
- Black and Ink Limits: 100% K for fine text; rich black at C40–60 M30–40 Y30–40 K100; total area coverage (TAC) ≤280%–300% (kept toward the lower end on absorbent uncoated fibers to prevent show-through and slow drying).
- Trim Geometry: 3 mm (0.118 in) bleed per side, ≥3 mm (0.118 in) safety margin (≥4–5 mm / 0.157–0.197 in for bordered backs), and R3–R3.5 mm (0.118–0.138 in) rounded corners.
Production Steps and Matte Sealing Trade-Offs
- Prepress Separation and TAC Reduction: Convert artwork to CMYK (plus separate spot channels if used) and curve midtones to compensate for higher dot gain on uncoated fibers. Keep fine text at 100% K and cap total ink density at ≤280%–300%.
- Stock Selection and Grain Alignment: Confirm the gsm and Cover LB specification for the target stiffness, verifying that surface sizing allows clean ink and graphite adhesion without excessive feathering.
- Offset Printing and Ink Set: Print on sheet-fed offset presses with extended drying intervals or IR/powder-free set controls so absorbed ink cures without transferring to the back of the next sheet.
- Sealing Decision (Bare vs. Matte):
- Unsealed (Bare): Preserves full paper tooth for pencil graphite, ballpoint ink, and dry stamps. Leaves dark solid areas vulnerable to edge rub and ink transfer during handling.
- Matte Sealing / Knockouts: Anti-scuff matte finishes suit dark artwork by protecting against surface rub, but full-bleed film lamination blocks pencil and smears water-based pens. If protection is needed on a writeable deck, restrict sealing to non-writeable backs or knock out the coating over designated writing fields.
- Die-Cutting and Corner Rounding: Die-cut decks to the project's custom trim dimensions with R3–R3.5 mm (0.118–0.138 in) corners, maintaining ≥3 mm (0.118 in) safety (≥4–5 mm / 0.157–0.197 in on bordered backs).
Sign-Off Criteria
Before approving a production run, verify the following conditions on physical press proofs or unlaminated stock samples:
- Direct Writeability: Ballpoint pen, #2 graphite pencil, and standard marker write cleanly on the designated zones without skipping, beading, or bleeding through to the reverse side.
- Shadow and Midtone Separation: Gradients and dark areas retain detail under uncoated dot gain, with TAC held ≤280%–300% and no ink set-off onto adjacent sheets.
- Surface Rub Tolerance: Unsealed dark faces and edges withstand normal deck collation without visible scuffing or pigment transfer.
- Trim and Margin Registration: Artwork clears the 3 mm (0.118 in) bleed, ≥3 mm (0.118 in) safety (≥4–5 mm / 0.157–0.197 in for bordered backs), and R3–R3.5 mm (0.118–0.138 in) corner dies.
Failure Modes and Mitigations
| Failure Mode | Physical Cause | Mitigation |
|---|---|---|
| Muddy shadows and plugged midtones | Uncoated fibers absorb wet ink laterally, increasing dot gain beyond coated press curves. | Apply uncoated CMYK separation profiles and cap TAC at ≤280%–300%. |
| Muted dark tones and visible scuffing | Ink sinks into open pores instead of sitting on a smooth topcoat, leaving pigment exposed to friction. | Avoid large unsealed dark solids on writeable faces, or use anti-scuff matte sealing on non-writeable backs. |
| Pen skipping or graphite failure | Film lamination or heavy full-bleed varnish seals off paper tooth and repels ink/graphite. | Leave writeable cards bare or apply spot knockouts over writing fields. |
| Marker feathering or show-through | Thin or loosely sized stock wicks solvent/water-based marker ink through the sheet. | Step up board weight (e.g., 350–400 gsm) or specify a tighter-sized cotton-blend sheet. |
| Uneven borders after die-cutting | Tight border artwork shifts visibly within standard sheet-fed die tolerances. | Maintain ≥4–5 mm (0.157–0.197 in) safety margins on all bordered backs. |
Parent guide Card Stocks and Paper Core Construction